Steam oxidation resistance comparison of several silicon carbide refractories at elevated temperatures
Wang Jiaping, Zhu Chong, Wu Jiguang, Huang Zhigang, Lyu Chunjiang
Refractories . 2022, (4): 351 -355 .  DOI: 10.3969/j.issn.1001-1935.2022.04.017