Effect of potassium fluorozirconate addition on properties of fly ash based cordierite ceramics
Li Jiayi, Liu Yangqiao, Chang Qibing, Gu Yajie, Sun Shengrui, Sun Ke, Chang Xinglan, Xi Shuang
Refractories . 2022, (6): 461 -466 .  DOI: 10.3969/j.issn.1001-1935.2022.06.001