Pore structure and performance of tabular corundum aggregates
Wu Pei, Han Bingqiang, Wei Jiawei, Wang Huijun
Refractories . 2022, (6): 481 -484 .  DOI: 10.3969/j.issn.1001-1935.2022.06.005