Wettability of silica sol modified multilayer graphene
Yu Baisong, Zhu Yening, Li Yangzhe, Su Yuqing, Wei Juncong, Tu Junbo, Wang Yilong
Refractories . 2022, (
6
): 523 -526 . DOI: 10.3969/j.issn.1001-1935.2022.06.014