Research progress of infrared radiation coatings for industrial kilns
Wu Qi, Wang Guangyang, Sun Yiran, Wang Xueqing, Sang Shaobai, Wang Qinghu, Li Yawei
Refractories . 2022, (
6
): 543 -547 . DOI: 10.3969/j.issn.1001-1935.2022.06.019