Corrosion of basic refractories for glass tanks using petrol coke and countermeasures
Wang Jiezeng, Liu Zhao, Xu Linlin, Chen Songlin, Liu Xijun
Refractories . 2023, (1): 50 -54 .  DOI: 10.3969/j.issn.1001-1935.2023.01.011