Effect of chromium addition on properties of corundum refractories
Li Jian, Yu Jingkun, Wen Tianpeng, Liu Zhaoyang
Refractories . 2023, (1): 55 -58 .  DOI: 10.3969/j.issn.1001-1935.2023.01.012