In-situ formed ceramic bonded Ti(C,N) composites and their properties
Zou Qiliang, Deng Chengji, Dong Bo, Ding Jun, Zhu Wanzheng, Wang Zhoufu, Zhu Hongxi, Wang Lin, Yu Chao
Refractories . 2023, (2): 93 -98 .  DOI: 10.3969/j.issn.1001-1935.2023.02.001