Analysis of corrosion mechanism of slag-line refractories of ZrO
2
-C submerged entry nozzles
Tian Chen, Zhi Jianjun, Gan Feifang, Fan Zhengjie, Gao Hua, Yuan Lei, Liu Guoqi, Yu Jingkun, Li Hongxia
Refractories . 2023, (
2
): 113 -116 . DOI: 10.3969/j.issn.1001-1935.2023.02.005