Modification of flake graphite with magnesium hydroxide by hydrothermal method
Zhou Ruiqi, Fan Huilin, Wang Zhiming, Cai Weijie, Duan Hongjuan, Zhang Haijun
Refractories . 2023, (
2
): 117 -120 . DOI: 10.3969/j.issn.1001-1935.2023.02.006