Preparation of SiC from organosilicon slurry solid waste
Wu Bowen, Wang Shuai, Guo Xiaolin, Xing Pengfei, Song Ailin, Zhuang Yanxin
Refractories . 2023, (2): 161 -165 .  DOI: 10.3969/j.issn.1001-1935.2023.02.016