Corundum-mullite porous materials printed by direct ink writing
Zhu Kai, Yang Daoyuan, Wang Meijiao, Yang Lianghua, Zhao Xiang, Chen Junhuan, Yuan Huiyu
Refractories . 2023, (
3
): 200 -204 . DOI: 10.3969/j.issn.1001-1935.2023.03.004