Effect of microsilica addition on properties of Al 2O 3-SiO 2 spraying mix
Cai Wei, Ju Maoqi, Chen Jinfeng, Cong Peiyuan
Refractories . 2023, (3): 241 -244 .  DOI: 10.3969/j.issn.1001-1935.2023.03.012