Research progress on effect of raw material characteristics on sintering densification of magnesium aluminate spinel
Wang Jianbin, Wang Zhanmin, Feng Haixia, Liu Jun, Han Yihui, Pan Yuanshuai
Refractories . 2023, (
3
): 259 -264 . DOI: 10.3969/j.issn.1001-1935.2023.03.016