Research progress on preparation of silicon nitride by catalytic nitridation
Wang Xin, Wang Junkai, Huang Zhen-xia, Meng Hao, Wang Yifei, Wen Yanke
Refractories . 2023, (
3
): 265 -269 . DOI: 10.3969/j.issn.1001-1935.2023.03.017