Preparation and properties of porous ceramics from limestone tailings
Yu Chao, Yang Xinyu, Chen Bo, Deng Chengji, Lyu Zhijiang, Dong Bo, Chen Yufeng, Ding Jun, Zhu Hongxi
Refractories . 2023, (4): 281 -285 .  DOI: 10.3969/j.issn.1001-1935.2023.04.002