Preparation of insulation materials from waste mullite-cordierite kiln furniture
Gao Chaochao, Xu Yanheng, Liu Mingyong, Wei Haichao, Zhou Ruxian, Liu Qiyun, Wang Rui, Min Xin, Huang Zhaohui
Refractories . 2023, (4): 343 -346 .  DOI: 10.3969/j.issn.1001-1935.2023.04.014