Application progress of h-BN in refractories and high temperature ceramics for metallurgy
He Yuanhang, Qian Fan, Guo Hairong, Li Hualong, Lu Yue, Liu Guoqi, Li Hongxia
Refractories . 2023, (4): 360 -364 .  DOI: 10.3969/j.issn.1001-1935.2023.04.018