Effect of heat treatment temperature on properties of SiC-MgAl
2
O
4
-Al composites
Sun Honggang, Li Hongxia, Si Yaochen, Du Yihao, Zhao Shixian, Shang Xinlian, Xia Miao
Refractories . 2023, (
5
): 390 -396 . DOI: 10.3969/j.issn.1001-1935.2023.05.004