Effect of sintering agent on properties of calcium zirconate materials
Lu Yue, Liu Guoqi, Yang Wengang, Yan Pengfei, Ma Weikui, Li Hongxia
Refractories . 2023, (
5
): 407 -411 . DOI: 10.3969/j.issn.1001-1935.2023.05.007