Corrosion behavior of slags with different basicities to corundum spinel castables
Yang Zongyuan, Wang Jing-ran, Wang Tong, Zhang Jinhua, Han Bingqiang, Ni Yue'e, Ke Changming
Refractories . 2024, (1): 13 -18 .  DOI: 10.3969/j.issn.1001-1935.2024.01.003