Dissolution behavior of waste high-alumina bricks in LF refining slag
Mu Xin, Jia Yi, Liu Chunyang, Chai Guangwei, Yu Wuming, Du Chuanming, Ma Beiyue
Refractories . 2024, (1): 25 -29 .  DOI: 10.3969/j.issn.1001-1935.2024.01.005