Effects of SiC polymer precursor and Zn composite powders on properties of Al 2O 3-C unfired slide plate materials
Liang Baoqing, Zhang Zhifeng, Wang Quanxi, Shang Junli, Li Hongyu, Zhao Chenrui, Zhao Yue
Refractories . 2024, (2): 137 -142 .  DOI: 10.3969/j.issn.1001-1935.2024.02.009