Effects of polypropylene fibers on thermal shock resistance of corundum-calcium hexaaluminate castables
Tian Pengdan, Wang Gang, Du Penghui, Feng Haixia, Wang Laiwen, Pan Yuanshuai
Refractories . 2024, (
3
): 208 -212 . DOI: 10.3969/j.issn.1001-1935.2024.03.006