Effect of boron oxide on mechanical properties of Al 2O 3-SiC-C castables
Shao Rongdan, Ju Maoqi, Cheng Shui-ming, Xia Changyong, Li Xuzhi, Zhang Han, Shan Jiangbo
Refractories . 2024, (3): 230 -233 .  DOI: 10.3969/j.issn.1001-1935.2024.03.010