Research progress on refractories for smelting reduction ironmaking process
Liu Ran, Liu Yanting, Gao Yanjia, Deng Yong
Refractories . 2024, (3): 251 -256 .  DOI: 10.3969/j.issn.1001-1935.2024.03.015