Effect of Ti-Si-Fe alloy addition on structure and properties of Si
3
N
4
bonded SiC refractories
Yao Luyan, Han Bingqiang, Zhang Jinhua, Ke Changming
Refractories . 2024, (
4
): 277 -283 . DOI: 10.3969/j.issn.1001-1935.2024.04.001