Effects of alumina particle size and zirconia powder extra-addition on sintering property of alumina granulated powder
Deng Jiang, Liu Xuexin, Li Wen, Zhang Ziyi, Yuan Wenjie
Refractories . 2024, (4): 307 -313 .  DOI: 10.3969/j.issn.1001-1935.2024.04.006