Influence of polyhydroxy saccharide binders on properties of Al 2O 3-SiC-C waterless taphole clay
Li Wenfeng, Shen Tianzi, Guo Huishi, Cao Jinjin, Kang Xiaoxu, Shi Kai, Kang Xiaoyang
Refractories . 2024, (4): 314 -318 .  DOI: 10.3969/j.issn.1001-1935.2024.04.007