Corrosion of corundum mullite bricks by slag from rotary kilns
Li Kunpeng, Yan Shuangzhi, Zhang Tao, Shi Pengkun, Feng Zhiyuan, Fan Muxu, Wang Han, Liu Pengcheng
Refractories . 2024, (
4
): 349 -353 . DOI: 10.3969/j.issn.1001-1935.2024.04.014