In-situ preparation and properties of ZrB 2 ceramics by boron/carbothermal reduction combined with hot pressing sintering
Liu Miaowei, Jia Quanli, Peng Xigao, Zhang Xiaohui, Zhang Ziying, Wang Haimei, Wang Jia
Refractories . 2024, (5): 381 -386 .  DOI: 10.3969/j.issn.1001-1935.2024.05.003