Effect of magnesite tailings powder on properties of MgO-SiO
2
castables
Zhang Xiaocun, Nie Jianhua, Liang Yonghe, Gao Dongsheng, Yan Wen, Yin Yucheng
Refractories . 2024, (
5
): 387 -392 . DOI: 10.3969/j.issn.1001-1935.2024.05.004