Effect of hydroxylated TiO 2 on properties of lightweight magnesia aggregates for cement kilns
Sun Gege, Li Guohua, Jiao Changfa, Tian Lin, Deng Shudan
Refractories . 2024, (5): 393 -399 .  DOI: 10.3969/j.issn.1001-1935.2024.05.005