Effects of rare earth oxides on low temperature solid phase synthesis of MgAl 2O 4 fibers
Guo Jiangpeng, Deng Changyu, Wang Xinyue, Chen Xinyu, Duan Hongjuan, Zhang Haijun
Refractories . 2024, (5): 410 -413 .  DOI: 10.3969/j.issn.1001-1935.2024.05.008