Phase composition and microstructure evolution of bauxite-based homogenized grogs during heating
马千里, 黄科, 徐德亭, 于仁红, 臧云飞, 马怀奇, 刘宇驰, 于晓蕊
Refractories . 2024, (6): 473 -479 .  DOI: 10.3969/j.issn.1001-1935.2024.06.003