Pressureless in-situ synthesis of MgAlON composites from spent slide bricks and spent MgO-C bricks
包强, 程翔, 邱桂博, 霍向涛, 王海娟, 郭敏, 张梅
Refractories . 2024, (6): 501 -505 .  DOI: 10.3969/j.issn.1001-1935.2024.06.008