Pressureless in-situ synthesis of MgAlON composites from spent slide bricks and spent MgO-C bricks
付琪琪, 赵庆彬, 张利新, 邓俊杰, 何旭辉, 陈留刚
Refractories . 2024, (6): 506 -512 .  DOI: 10.3969/j.issn.1001-1935.2024.06.009