Effect of Al 2O 3 content on hot mechanical properties of magnesium aluminate spinel
Fan Muxu, Shi Gan, Zhang Wei
Refractories . 2021, (1): 35 -39 .  DOI: 10.3969/j.issn.1001-1935.2021.01.008