Effect of Si 3N 4/Si 2N 2O multiphase powder on properties of Al 2O 3-SiC-C castables
Li Youqi, He Jian, Chen Junfeng, Zhang Jialiang, Li Zhengkun
Refractories . 2025, (1): 1 -7 .  DOI: 10.3969/j.issn.1001-1935.2025.01.001