Corrosion of high level radioactivity waste borosilicate liquid glass on chrome corundum refractories
Qu Xiaorui, Chen Liugang, Liu Ping, Gao Guangze, Fu Qiqi, Zhang Lixin
Refractories . 2025, (1): 31 -37 .  DOI: 10.3969/j.issn.1001-1935.2025.01.006