Study on infrared radiation coatings based on Si-Fe tailings slag and their performance
Zhou Tao, Fu Lyu-ping, Yang Shuang, Chen Ding, Zhang Meijie, Huang Ao, Gu Huazhi
Refractories . 2025, (
2
): 123 -127 . DOI: 10.3969/j.issn.1001-1935.2025.02.006