Preparation and high-temperature resistance of Fe 2O 3-SiO 2 composite aerogel materials
Hou Jianye, Zhang Zhonglun, Fu Xiaoqing, Wang Mingming, Liu Zhensen
Refractories . 2025, (2): 133 -137 .  DOI: 10.3969/j.issn.1001-1935.2025.02.008