Preparation of high performance sintered magnesia by utilizing salt lake brine
Zhou Yujun, Tang Dacai, Wen Tianpeng, Yu Jingkun
Refractories . 2025, (2): 162 -166 .  DOI: 10.3969/j.issn.1001-1935.2025.02.013