Property optimization of magnesium aluminate spinel based on orthogonal design
Cheng Qingnan, Qian Kun, Chen Bo, Wang Jianjun, Liu Kui
Refractories . 2025, (
3
): 198 -202 . DOI: 10.3969/j.issn.1001-1935.2025.03.003