Effects of waste high alumina sphere powder on performance of mullite-alumina-quartz multiphase materials
Lyu Zhenfei, Fan Mengke, Cao Yukun, Li Xihu, Ke Yanghui, Zhang Xuejia, Wang Xuekai, Shen Xiulin, Zhang Xiaoguang
Refractories . 2025, (4): 323 -329 .  DOI: 10.3969/j.issn.1001-1935.2025.04.009