Microstructure and thermal shock resistance of corundum-spinel castables containing nano-CaCO
3
Tan Dan, Wang Jingran, Zhang Jinhua, Ni Yue’e, Han Bingqiang
Refractories . 2025, (
4
): 330 -336 . DOI: 10.3969/j.issn.1001-1935.2025.04.010