Performance research and process optimization of spinel-carbon stopper heads for continuous casting
Fang Wenji, Pan Lei, Gao Zhi, Wang Zuochuang, Yang Qin, Ma Beiyue
Refractories . 2025, (
4
): 340 -344 . DOI: 10.3969/j.issn.1001-1935.2025.04.012