Effect of Al(H 2PO 4) 3 and SiO 2 sol on microstructure and properties of zirconia-based coatings
Zhong Xing-yu, Zhao Shixian, Wang Gang, Li Hongyu, Li Lingfeng, Liang Pengpeng, Tian Pengdan, Li Hongxia, Liu Xue-zhi
Refractories . 2025, (5): 386 -390 .  DOI: 10.3969/j.issn.1001-1935.2025.05.004