Preparation and properties of SiO 2-Al 2O 3 composite aerogels
Wang Zhizheng, Guo Yuxiang, Wang Xin, Yang Bo, Sun Peisong, Zhang Fengchuang
Refractories . 2025, (5): 391 -397 .  DOI: 10.3969/j.issn.1001-1935.2025.05.005