Preparation of porous ceramics by impregnating mullite precursor with activated carbon and their perfor-mance
Xi Jianfei, Zhang Ling, Niu Shunan, Luo Shitong, Duan Mingjun
Refractories . 2025, (5): 413 -421 .  DOI: 10.3969/j.issn.1001-1935.2025.05.008